Printing Parameters
Description | Data | Desciption | Data |
Nozzle Temperature | 190—230℃ | Nozzle Size | 0.2,0.4,0.6,0.8mm |
Printing Platform Material | - | Printing Platform Surface Treatment | Add glue according to material |
Bottom Value Sparation Distance | 0.4-0.6 | Withdrawal Distance | 5mm |
Environment Temperature | Room temperature | Withdrawal Speed | 50mm/s |
Recommended Support Material | - | Drying Temperature | 50℃ |
Printing Speed | 40--300 mm/s | Cooling Fan | 100% |
- |
Physical Properties
Properties | Testing method | Value |
Density | ISO 1183 | 1.31g/cm3 |
Melt Flow Index | 210℃,2.16kg 39.4±3.2g/min | |
20g/10min |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transsition | DSC, 10℃/min | 61℃ | |
Melting Temperature | DSC, 10℃/min | 163℃ | |
Decomposition Temperature | / | ≥374℃ | |
Vicat Softening Temperature | ISO 306, GB/T 1040 | 63℃ | |
Heat Distortion Temperature | ISO75 | 0.45Mpa/58℃, 1.80Mpa/52℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ISO527, GB/T 1040 | 32Mpa |
Elongation at break | ISO527, GB/T 1040 | 6.8% |
Flexural Strength | ISO178, GB/T 9341 | 55Mpa |
Flexural Modulus | ISO178, GB/T 9341 | 2456Mpa |
Impact Strength with Notched | ISO179, GB/T 1043 | 6.73KJ/㎡ |
Impact Strength without Notched | ISO179, GB/T 1043 | 19.2KJ/㎡ |
Printing Parameters
Description | Data | Desciption | Data |
Nozzle Temperature | 190—230℃ | Nozzle Size | 0.2,0.4,0.6,0.8mm |
Printing Platform Material | - | Printing Platform Surface Treatment | Add glue according to material |
Bottom Value Sparation Distance | 0.4-0.6 | Withdrawal Distance | 5mm |
Environment Temperature | Room temperature | Withdrawal Speed | 50mm/s |
Recommended Support Material | - | Drying Temperature | 50℃ |
Printing Speed | 40--300 mm/s | Cooling Fan | 100% |
- |
Physical Properties
Properties | Testing method | Value |
Density | ISO 1183 | 1.31g/cm3 |
Melt Flow Index | 210℃,2.16kg 39.4±3.2g/min | |
20g/10min |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transsition | DSC, 10℃/min | 61℃ | |
Melting Temperature | DSC, 10℃/min | 163℃ | |
Decomposition Temperature | / | ≥374℃ | |
Vicat Softening Temperature | ISO 306, GB/T 1040 | 63℃ | |
Heat Distortion Temperature | ISO75 | 0.45Mpa/58℃, 1.80Mpa/52℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ISO527, GB/T 1040 | 32Mpa |
Elongation at break | ISO527, GB/T 1040 | 6.8% |
Flexural Strength | ISO178, GB/T 9341 | 55Mpa |
Flexural Modulus | ISO178, GB/T 9341 | 2456Mpa |
Impact Strength with Notched | ISO179, GB/T 1043 | 6.73KJ/㎡ |
Impact Strength without Notched | ISO179, GB/T 1043 | 19.2KJ/㎡ |