Availability: | |
---|---|
Printing Parameters
Description | Data | Desciption | Data |
Nozzle Temperature | 190—230℃ | Heated bed Temperature | 50-60℃ |
Printing Platform Material | Soft Magnetic Sticker | Printing Platform Surface Treatment | No Processing Required |
Bottom Value Sparation Distance | 0.4-0.6 | Withdrawal Distance | 1mm |
Environment Temperature | Room temperature | Withdrawal Speed | 50mm/s |
Recommended Support Material | PVA | Drying Temperature | 50℃ |
Printing Speed | 40--250 mm/s | Cooling Fan | 100% |
Suitable for all FDM 3D Printers / 3D Printing Machines |
Physical Properties
Properties | Testing method | Value |
Density | ASTM D792 | @23℃ 1.25g/cm3 |
Melt Flow Index | ASTM D1238 | 190℃/2.16kg 9g/10min |
Flame Properties
Properties | Testing method | Value |
Flame Retardance | UL94 | @1.5mm HB |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transsition | ASTM D7426 | @10℃/min 60.9℃ | |
Melting Temperature | ASTM D7426 | @10℃/min 164℃ | |
Decomposition Temperature | ASTM E2402 | @20℃/min ≥364℃ | |
Cofficient of Thermal Expansion | ASTM E831 | 101×10-06 ㎛(m· ℃) | |
Shrinking Percentage | ASTM D955 | @23℃ 0.1-0.3% | |
Vicat Softening Temperature | ASTM D1525 | 5kg,50℃/h 54℃ | |
Heat Distortion Temperature | ASTM D648 | 0.45Mpa/53℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ASTM D638 | @50mm/min 60.6Mpa |
Elongation at break | ASTM D638 | @50mm/min 6.3% |
Flexural Strength | ASTM D790 | @2mm/min 65Mpa |
Flexural Modulus | ASTM D790 | @2mm/min 1895Mpa |
Charpy Impact Strength with Notched | ASTM D256 | @3.2mm 33J/㎡ |
Young Modulus | ASTM D638 | @1mm/min 2760Mpa |
Chemical Resistance
Item | Grade |
Weak Acids Affect pH3-6 | Good |
Strong Acids Affect pH<3 | Poor |
Weak Base Affect pH8-10 | Good |
Strong Base Affect pH>10 | Poor |
Deionized Water | Good |
Athyl Alcohol | Average |
Acetone | Poor |
Gasoline | Good |
Ether | Good |
Printing Parameters
Description | Data | Desciption | Data |
Nozzle Temperature | 190—230℃ | Heated bed Temperature | 50-60℃ |
Printing Platform Material | Soft Magnetic Sticker | Printing Platform Surface Treatment | No Processing Required |
Bottom Value Sparation Distance | 0.4-0.6 | Withdrawal Distance | 1mm |
Environment Temperature | Room temperature | Withdrawal Speed | 50mm/s |
Recommended Support Material | PVA | Drying Temperature | 50℃ |
Printing Speed | 40--250 mm/s | Cooling Fan | 100% |
Suitable for all FDM 3D Printers / 3D Printing Machines |
Physical Properties
Properties | Testing method | Value |
Density | ASTM D792 | @23℃ 1.25g/cm3 |
Melt Flow Index | ASTM D1238 | 190℃/2.16kg 9g/10min |
Flame Properties
Properties | Testing method | Value |
Flame Retardance | UL94 | @1.5mm HB |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transsition | ASTM D7426 | @10℃/min 60.9℃ | |
Melting Temperature | ASTM D7426 | @10℃/min 164℃ | |
Decomposition Temperature | ASTM E2402 | @20℃/min ≥364℃ | |
Cofficient of Thermal Expansion | ASTM E831 | 101×10-06 ㎛(m· ℃) | |
Shrinking Percentage | ASTM D955 | @23℃ 0.1-0.3% | |
Vicat Softening Temperature | ASTM D1525 | 5kg,50℃/h 54℃ | |
Heat Distortion Temperature | ASTM D648 | 0.45Mpa/53℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ASTM D638 | @50mm/min 60.6Mpa |
Elongation at break | ASTM D638 | @50mm/min 6.3% |
Flexural Strength | ASTM D790 | @2mm/min 65Mpa |
Flexural Modulus | ASTM D790 | @2mm/min 1895Mpa |
Charpy Impact Strength with Notched | ASTM D256 | @3.2mm 33J/㎡ |
Young Modulus | ASTM D638 | @1mm/min 2760Mpa |
Chemical Resistance
Item | Grade |
Weak Acids Affect pH3-6 | Good |
Strong Acids Affect pH<3 | Poor |
Weak Base Affect pH8-10 | Good |
Strong Base Affect pH>10 | Poor |
Deionized Water | Good |
Athyl Alcohol | Average |
Acetone | Poor |
Gasoline | Good |
Ether | Good |