Description | Data | Desciption | Data |
Nozzle Temperature | 265—290℃ | Heated bed Temperature | 80℃ |
Nozzle Diameter | ≥0.4 mm | Printing Platform | Add glue according to Materials |
Printing Speed | 40-300 mm/s | Cooling fan | Not required |
Suitable for all FDM 3D Printers / 3D Printing Machines |
Physical Properties
Properties | Testing method | Value |
Density | ISO 1183-1 | 1.20g/cm3 |
Melt Flow Index | ISO 1133 | 6g/10min |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transition | ISO 11357 | 177℃ | |
Melting Temperature | ISO 11357 | 219℃ | |
Decomposition Temperature | / | 458℃ | |
Vicat Softening Temperature | ISO 306 | / | |
Heat Distortion Temperature | ISO 72 | 0.45Mpa 1.80Mpa | 175℃ 71℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ISO 527 | 113.5Mpa |
Elongation at break | ISO 527 | 1.15% |
Flexural Strength | ISO 178 | 168Mpa |
Flexural Modulus | ISO 178 | 9142Mpa |
Charpy Impact Strength with Notched | ISO 179 | 8.24KJ/㎡ |
Charpy Impact Strength without Notched | ISO 179 | 29.27KJ/㎡ |
Printing Parameters
Description | Data | Desciption | Data |
Nozzle Temperature | 265—290℃ | Heated bed Temperature | 80℃ |
Nozzle Diameter | ≥0.4 mm | Printing Platform | Add glue according to Materials |
Printing Speed | 40-300 mm/s | Cooling fan | Not required |
Suitable for all FDM 3D Printers / 3D Printing Machines |
Physical Properties
Properties | Testing method | Value |
Density | ISO 1183-1 | 1.20g/cm3 |
Melt Flow Index | ISO 1133 | 6g/10min |
Thermal Performance
Properties | Testing Method | Value | |
Glass Transition | ISO 11357 | 177℃ | |
Melting Temperature | ISO 11357 | 219℃ | |
Decomposition Temperature | / | 458℃ | |
Vicat Softening Temperature | ISO 306 | / | |
Heat Distortion Temperature | ISO 72 | 0.45Mpa 1.80Mpa | 175℃ 71℃ |
Mechanical Performance
Printing Direction | Testing Standard | Data |
Tensile Strength | ISO 527 | 113.5Mpa |
Elongation at break | ISO 527 | 1.15% |
Flexural Strength | ISO 178 | 168Mpa |
Flexural Modulus | ISO 178 | 9142Mpa |
Charpy Impact Strength with Notched | ISO 179 | 8.24KJ/㎡ |
Charpy Impact Strength without Notched | ISO 179 | 29.27KJ/㎡ |