As a professional PA6 supplier, we deliver engineering-grade nylon materials that exceed industry standards. This nylon 3d printer filament combines advanced processing capabilities with exceptional mechanical properties.
Processing temperature: 250-280°C
Premium mechanical strength: 59MPa tensile, 108MPa flexural
Industrial heat resistance up to 458°C
ISO-certified manufacturing process
Consistent dimensional accuracy: ≥0.4mm nozzle compatibility
Our high strength 3D printing material serves:
Custom nylon parts manufacturing
Industrial nylon 3D printing projects
Mechanical parts 3D printing needs
Engineering grade filament applications
✓ Certified quality control
✓ Technical support
✓ Competitive pricing
✓ Stable supply chain
Contact our engineering team for complete specifications and processing guidelines. Sample testing available for qualified industrial projects.
Printing Parameters
| Description | Data | Desciption | Data | 
| Nozzle Temperature | 250—280℃ | Heated bed Temperature | 80℃ | 
| Nozzle Diameter | ≥0.4 mm | Printing Platform | Add glue according to Materials | 
| Printing Speed | 40--300 mm/s | Cooling fan | On | 
| Suitable for all FDM 3D Printers / 3D Printing Machines | |||
Physical Properties
| Properties | Testing method | Value | 
| Density | ISO 1183-1 | 1.13g/cm3 | 
| Melt Flow Index | ISO 1133 | 18 g/10min | 
Thermal Performance
| Properties | Testing Method | Value | |
| Glass Transition | ISO 11357 | 184℃ | |
| Melting Temperature | ISO 11357 | 220℃ | |
| Decomposition Temperature | / | 458℃ | |
| Vicat Softening Temperature | ISO 306 | / | |
| Heat Distortion Temperature | ISO 72 | 0.45Mpa 1.80Mpa | ℃ ℃ | 
Mechanical Performance
| Printing Direction | Testing Standard | Data | 
| Tensile Strength | ISO 527 | 59Mpa | 
| Elongation at break | ISO 527 | 2% | 
| Flexural Strength | ISO 178 | 108Mpa | 
| Flexural Modulus | ISO 178 | 2535Mpa | 
| Charpy Impact Strength with Notched | ISO 179 | KJ/㎡ | 
| Charpy Impact Strength without Notched | ISO 179 | KJ/㎡ | 
As a professional PA6 supplier, we deliver engineering-grade nylon materials that exceed industry standards. This nylon 3d printer filament combines advanced processing capabilities with exceptional mechanical properties.
Processing temperature: 250-280°C
Premium mechanical strength: 59MPa tensile, 108MPa flexural
Industrial heat resistance up to 458°C
ISO-certified manufacturing process
Consistent dimensional accuracy: ≥0.4mm nozzle compatibility
Our high strength 3D printing material serves:
Custom nylon parts manufacturing
Industrial nylon 3D printing projects
Mechanical parts 3D printing needs
Engineering grade filament applications
✓ Certified quality control
✓ Technical support
✓ Competitive pricing
✓ Stable supply chain
Contact our engineering team for complete specifications and processing guidelines. Sample testing available for qualified industrial projects.
Printing Parameters
| Description | Data | Desciption | Data | 
| Nozzle Temperature | 250—280℃ | Heated bed Temperature | 80℃ | 
| Nozzle Diameter | ≥0.4 mm | Printing Platform | Add glue according to Materials | 
| Printing Speed | 40--300 mm/s | Cooling fan | On | 
| Suitable for all FDM 3D Printers / 3D Printing Machines | |||
Physical Properties
| Properties | Testing method | Value | 
| Density | ISO 1183-1 | 1.13g/cm3 | 
| Melt Flow Index | ISO 1133 | 18 g/10min | 
Thermal Performance
| Properties | Testing Method | Value | |
| Glass Transition | ISO 11357 | 184℃ | |
| Melting Temperature | ISO 11357 | 220℃ | |
| Decomposition Temperature | / | 458℃ | |
| Vicat Softening Temperature | ISO 306 | / | |
| Heat Distortion Temperature | ISO 72 | 0.45Mpa 1.80Mpa | ℃ ℃ | 
Mechanical Performance
| Printing Direction | Testing Standard | Data | 
| Tensile Strength | ISO 527 | 59Mpa | 
| Elongation at break | ISO 527 | 2% | 
| Flexural Strength | ISO 178 | 108Mpa | 
| Flexural Modulus | ISO 178 | 2535Mpa | 
| Charpy Impact Strength with Notched | ISO 179 | KJ/㎡ | 
| Charpy Impact Strength without Notched | ISO 179 | KJ/㎡ |